Abstract

The defects destroy the integrity of the enamel, and the paper examines the influence of the physical-mechanical and corrosion properties of frits and heat treatment on the defectiveness of the enamel coating. The surface defects were scanned by electron microscope. It has been established that the defectiveness of enamel coatings depends on the melting index, temperature coefficient of linear expansion, surface tension of the frits, and heat treatment conditions. When burning rate of the enamel coating decreases, the fine-meshed structure of the enamel changes, and the size of the defects decreases.

About the Authors

T. O. Soshina
Perm National Research Polytechnic University
Russian Federation

Cand Sc. (Eng)

Lysva branch, 2 Lenina St, 618900 Lysva



V. R. Mukhamadyarovа
Lysva Plant of Enameled Cookware JSC
Russian Federation
1 Metallistov St, 618909 Lysva


References

1. Lazutkina, O.R., Emalirovochnoe proizvodstvo [Enamel production], Ekaterinburg: UrFU, 2010, p. 127.

2. Solntsev, S.S., Zashchitnye tekhnologicheskie i tugoplavkie emali [Protective technological and refractory enamels], Moscow: Mashinostroenie, 1984, p. 256.

3. Lazutkina, O.R., Nizkotemperaturnye pokrovnye emali dlya stali i alyuminiya [lowtemperature coverslips enamels for steel and aluminum], Steklo i Keramika, 2008, No 2, pp. 32–33.

4. Volokitin, O.G., Osobennosti fiziko-khimicheskikh protsessov polucheniya vysokotemperaturnykh silikatnykh rasplavov [Features of physical and chemical processes of obtaining hightemperature silicate melts], Izvestiya VUZov. Khimiya i Khimicheskaya Tekhnologiya, 2013, V. 56, No 8, pp. 71–76.

5. Aleutdinov, A.D., Ustranenie defektov stekloemalevogo pokrytiya vozdeistviem sfokussirovannogo svetovogo izlucheniya [Removal of glass-enamelcovering defects using focused light radiation], Izvestiya VUZov. Fizika, 2013, V. 56, No 1–2, pp. 285–286.

6. Shalygina, O.V., Odnofritnye beznikelevye stekloemalevye pokrytiya, poluchaemye po tekhnologii POESTA [Single-fritted nickel-free glass-enamel coverings obtained by POESTA technology], Steklo i keramika, 2014, no 6, pp. 38–42.

7. Frits. Specifications: State Standard GOST P 52569–2006

8. Enamelled steel kitchen utensils. General specifications: State Standard GOST P 24788–2001.


Review

For citations:


Soshina T.O., Mukhamadyarovа V.R. On the defects of enamel coatings. Voprosy Materialovedeniya. 2018;(4(96)):145-150. (In Russ.) https://doi.org/10.22349/1994-6716-2018-96-4-145-150

Views: 728


ISSN 1994-6716 (Print)